Modded Ender 3 Neo (direct drive, dual 5015 fans, Bimetal heatbreak and hardened nozzle), custom marlin. Printing well all basic polymaker filaments, as PETG, PETG rCF08, PLA, TPU. Bought PA12-CF20, did temp tower (turned out pretty good - not bad), went with 270°. And here I did flowrate test and forgot to supervise the printer. No blob, no failure (hardware), but the result kinda confuses me. This is 8~20mm^3/s. Petg cf08 is 12 (stock value, prints well, iirc 15.5 was result of test there). Is it flow ratio bad, dryness, or normal behaviour for 40-50w heater with mk8 heatblock (neo radiator), and this amount of CF? Anything to change? Thanks!
Orca slicer, 0.2 standard process profile, with standard speeds of 30-40 first layer, 40 outer, 60 inner, 80 for basic stuff.
If any other specs/info needed - ask!