r/Prospecting • • 5d ago

What am I doing wrong

Post image

Not sure this is the place for this,

Found some rocks with gold in it. Crushed and panned what I could. There was still some black sand.

I tried melting it down today and this kept happening.

Is it not hot enough? Is it cooling too fast. Any suggestions or tips.

Using a propane forge to heat up. Also have a small propane torch i could try.

24 Upvotes

17 comments sorted by

23

u/Gold_Au_2025 5d ago

Looks like nowhere near enough heat.

7

u/OdensEye87 5d ago

The pic is a few minutes after. It looked like a puddle in the cruicible. But the gold stayed seperate. Ill try more heat

10

u/gold2019 5d ago

needs more borax and you need to get that temp up and hold it at 1980 degrees for 20 minutes min. borax will lower the melting point also add wheat flour yes i said it. wheat flour soda as as well.

4

u/OdensEye87 5d ago

Thank you. Ill try more and longer heat. Never heard of trying wheat flour. I have some so ill give it a go tomorrow

6

u/texascharley 5d ago

What are you doing period?

2

u/OdensEye87 5d ago

I crush and panned the ore as best as I can(new to this) still some black sand in it.

Put it in a crucible in my propane forge and let it get glowing hot for a bit. Looked like a puddle in it. The take it out and try to pour it into a mold. It doesnt like to come out. I do have a small propane torch I cab try to use as well

I add borax to it before and during the heating.

I got some peices out the are decent size. But seems lots wont pour for me

1

u/Dr_Daze 24m ago

If it didnt want to come out its either not enough heat or not enough borax/flux mixture

4

u/for-a-nickel-I-will 5d ago

What were your fluxes. If it's placer gold dust in black sand it is best removed with clean clear glass and borax to thin it and potassium nitrate to oxidize the iron and force it into the glass. Depending on how much gold is in the sample and how small the particles are will dictate if you need a collector metal like lead oxide better know and litheige. Bring up your heat steadily allowing the mix to boil slowly without boiling over once. Don't stir and once it's quit boiling turn the heat up till it's a bright hot red. Simmer at temp for 5 min. I use the green clay crucible because they are cheap so I can treat them as disposable. So once it's simmered out turn off your heat and leave it to cool. Take it out and carefully break the crucible apart and the gold should be at the bottom. Keep all the slag and crush and pan it making sure it all collected. If you use a collector metal you will then have to use a cupel to remove the lead.
Do you know the karot ? What are the impurities? Copper silver tin etc.

3

u/OdensEye87 5d ago

Seems I shoukd do some more research.

There is some small flakes and lots of flour. I do think I didnt heat it enough. I was also working in my shop outside. It was maybe 5 degrees c in there.

3

u/for-a-nickel-I-will 5d ago

I gave you the exact way to get fine gold from black sand. If that's not what your doing then this will still work kinda. But if your dealing with sulfides or oxides of Gold and silver you will need to adjust your flux. You will find all kinds of different recipes from different people. Most of which will complicate the melt more than it needs to be. Mount baker mining guy is the prime example of some one that just don't get it. He makes it so much more difficult than need be. What you really need is the proper equipment and tools. I have 40 years of refining under my belt and I was taught by a 70 year old man raised on the Comstock when I was 20. Dm me if you want more info glad to help

2

u/rockphotos 5d ago

Looks like you're trying to smelt in a cupel and not in a crucible.

Crucible smelt first to get a button

Cupeling is for pulling base metals out of your button to get your refined prill.

Cupels have a small capacity and can't pull all the slag off directly.

2

u/SnooLentils5747 5d ago

get yourself an oxypropane torch, like for brazing. trust me

2

u/TheBugDude 5d ago

It takes a surprising amount of heat the first time you melt gold. Its not usually a "quick" experience. It will look like a pool of glowing yellow/white hot liquid that flows and jiggles around when bumped or stirred. Its not "super easy" to vaporize gold once you realize its melted too, but not impossible either. Just realize that when its melted and totally liquid, its time to pour. Pour into a heated (hot hot) mold, keep the torch on the dish while you do that.

I would use baked ("anhydrous") borax powder and junk glass as my flux.

1

u/Original-Concert-456 4d ago

Hmm. I have so much black sand from panning also. Always planned on doing this. Never had the chance. I was told to get a potato and gut it bake it in a fire wrapped in aluminum foil. Seemed to easy to be true

1

u/RustyMcGhost 5d ago

Make sure you are using MAPP gas rather than butane or propane, use less borax, and apply concentrated heat. Do not use too close, but ensure it is far enough back that it is not blowing your gold around; also, never use acetylene gas, as it gets hot enough to vaporize gold or silver. Additionally, your mold needs to be preheated, and you should add a drop of WD-40 to it.