r/snapmaker • u/tofu_snufkin • 2d ago
Solved Top and bottom surface problems.

Snapmaker U1 and Orca Slicer. Lines are too far apart on bottom surfaces, blobbing and vfa-looking artifacts on top surfaces.
Plate: Biqu Cryogrip Glacier
Filament: eSun PLA Matte Milky White
Settings for filament are Generic PLA Preset but flow ratio adjusted to 0.96, max volumetric speed set to 15, side fan turned off and bed temperature set to 60 degrees with cooling turned off for first 2 layers.
Process settings are 0.20 Standard with "textured cool plate" and sparse infill set to cubic.
3
Upvotes




3
u/tofu_snufkin 2d ago
EDIT: Fixed.
Biqu Cryogrip Glacier plate needs manual z-offset adjustment on Snapmaker U1. Will be fine tuning top surface after that.
2
u/Moist_Show1750 2d ago
Interesting, it looks underextruded in one face and overextruded in the other. perhaps Z offset needs to be calibrated so the bottom is extruded well and then reduce flow rate so that the top layer is not overextrduded?
2
u/Lordrew 2d ago
I also had first layer issues with biqu, for me first layer needs to be 0.2 with offset of -0.02 , you can try s simple cube 60x60x0.25, also try auto leveling before print and see the mesh